Engineering Overview
The SANSO Steel Coil Cut to Length Line (CTL Machine) converts heavy master steel coils into stress-relieved, dead-flat metal sheets cut to exact customer dimensions. Engineered with 17-roll or 21-roll 4-Hi/6-Hi precision levelers and closed-loop AC servo length control, SANSO CTL lines achieve ±0.5 mm length accuracy and ≤1.5 mm/m flatness across 0.3 mm to 16.0 mm thicknesses.
Key Engineering Features & Advantages
- High-Precision Multi-Roll Leveler: Hardened alloy work rolls (HRC 58–62) with adjustable backup flights eliminate coil set, cross-bow, edge waves, and center buckle completely.
- Servo Flying Shear or Stop-Start Hydraulic Shear: Choose high-speed rotary/flying shear (up to 80–100 m/min) for continuous thin-gauge throughput, or heavy-duty hydraulic guillotine shear for thick plates up to 16 mm.
- Automated Pneumatic Sheet Stacker: Scratch-free air-cushion or drop-frame stacking aligns cut blanks into neat packs ready for strapping and dispatch without manual handling.
- Optional Edge Trimming Unit: Integrated inline side trimmer removes rough mill edges before cross-shearing to guarantee squareness within ±1.0 mm diagonal tolerance.
Technical Specifications
| Model | Strip Thickness (mm) | Max Width (mm) | Max Coil Weight (T) | Shear Type | Line Speed (m/min) |
|---|
| SS-CTL1300 Fly | 0.3 – 2.5 | 1300 | 15 | Servo Flying / Rotary Shear | 60 – 80 |
| SS-CTL1600 Med | 0.5 – 4.0 | 1650 | 20 | NC Servo / Hydraulic Shear | 35 – 50 |
| SS-CTL1600 Heavy | 2.0 – 10.0 | 1650 | 25 | Heavy Hydraulic Guillotine | 20 – 35 |
| SS-CTL2000 Plate | 4.0 – 16.0 | 2000 | 25–30 | Heavy Plate Hydraulic Shear | 15 – 25 |
Process Flow & System Configuration
Coil Car → Hydraulic Uncoiler → Peeler & Snubber Roll → Pre-Leveler → Looping Bridge → Side Guide → Precision 17/21-Roll Leveler → Servo Length Measuring & Feeder → High-Speed Shear → Belt Conveyor → Automatic Pneumatic Stacker & Runout Table.
Frequently Asked Questions
What is the cutting accuracy of a SANSO cut to length line?
Standard SANSO CTL lines maintain ±0.5 mm length tolerance (at 2,000 mm sheet length) and ≤±1.0 mm diagonal accuracy via dual-encoder closed-loop servo control.
When should I choose a flying shear CTL machine over a stop-start hydraulic shear?
For thin-to-medium gauge coils (0.3–3.0 mm) requiring high output above 50 m/min, a servo flying shear eliminates stop-start marks and doubles productivity. For heavy structural plates (4–16 mm), a hydraulic guillotine shear offers maximum cutting force and lower capital cost.
Can SANSO combine slitting and cut-to-length in one coil processing line?
Yes, we build 2-in-1 combined slitting and cut-to-length lines for 0.5–6.0 mm steel coils where shop floor space is limited and multi-format production is required.