Contact Us
Coil Processing Equipment

Steel Coil Slitting Line (Precision Coil Slitter)

Precision steel coil slitting line engineered to uncoil, slit, tension, and recoil wide master steel coils into accurate narrow strips for ERW tube mills.

Model / Series
SS-SL1600 / SS-SL2000
Processing Capacity / Range
Coil Width 600–2000 mm · Max Coil Weight 10–25 Tons
Thickness / Wall Range
0.2–2.0 mm (Light) / 0.5–3.5 mm (Medium) / 2.0–6.0 mm (Heavy)
Max Line Speed / Output
0–150 m/min standard (up to 200 m/min high-speed)
Send Line Specifications
Technical Datasheet

Key Technical Parameters

Specification Item SANSO Engineering Standard
Model / Series SS-SL1600 / SS-SL2000
Processing Capacity / Range Coil Width 600–2000 mm · Max Coil Weight 10–25 Tons
Thickness / Wall Range 0.2–2.0 mm (Light) / 0.5–3.5 mm (Medium) / 2.0–6.0 mm (Heavy)
Max Line Speed / Output 0–150 m/min standard (up to 200 m/min high-speed)
Drive & Power Configuration AC Variable Frequency / DC Drive + Hydraulic Expansion
Applicable Materials / Grade CR Steel, HR Steel, Galvanized (GI), Stainless Steel, Silicon Steel, Aluminum, PPGI
Precision & Standards Width Tolerance ±0.05 mm · Slitting Burr ≤ 3% of Strip Thickness
Primary Applications ERW welded tube mill strip preparation, steel service centers, automotive stamping, transformer cores, roll forming

Engineering Overview

The SANSO Steel Coil Slitting Line is an integrated heavy-duty coil processing system engineered to slit master coils (up to 25 tons and 2000 mm width) into precision narrow steel strips required for ERW welded tube mills, C/Z purlin roll formers, and automotive stamping presses. Built with 90% in-house CNC machined housings and forged alloy tool-steel slitter arbors, the line maintains burr heights below 3% of strip thickness and width tolerances within ±0.05 mm at speeds up to 200 m/min.

Key Engineering Features & Advantages

  • Precision Slitter Head: Zero-clearance tapered roller bearings and hardened 42CrMo arbors minimize axial runout and deliver clean, burr-free strip edges essential for high-frequency ERW weld quality.
  • Dual-Head Exchangeable Slitter Option: Optional quick-change dual slitter heads allow offline knife setup while the line runs, reducing coil-width changeover time by up to 70%.
  • Uniform Recoiling Tension: Pneumatic felt pad and hydraulic tensioning rolls guarantee tightly wound, telescope-free slit coils across all strip strands regardless of coil crown variations.
  • Full PLC Automation: Siemens/Schneider PLC touchscreen synchronization controls uncoiler payoff, looping pit depth, slitter speed, scrap winder, and recoiler torque seamlessly.

Technical Specifications

ModelCoil Thickness (mm)Max Coil Width (mm)Max Coil Weight (T)Max Slitting Speed (m/min)Width Tolerance
SS-SL1300 Light0.2 – 2.0130015180±0.05 mm
SS-SL1600 Medium0.5 – 3.5165020150±0.05 mm
SS-SL1600 Heavy1.5 – 6.0165025100±0.10 mm
SS-SL2000 Heavy2.0 – 8.0200025–3080±0.10 mm

Process Flow & System Configuration

Coil Loading Car → Hydraulic Uncoiler → Pinch Roll & Peeler Table → 5-Roll Pre-Leveler → Crop Shear → Side Guides → Precision Slitter Head → Dual Scrap Winders → Looping Pit → Tension Stand & Separator → Hydraulic Recoiler → Discharge Coil Car & Turnstile.

Frequently Asked Questions

What strip edge burr tolerance does a SANSO steel coil slitting line achieve?

SANSO slitting lines hold slitting burr to ≤3% of strip thickness with strip width accuracy within ±0.05 mm on light-to-medium gauge coils, preventing edge mismatch during subsequent ERW tube welding.

How does coil slitting affect ERW welded tube mill quality?

Clean, parallel, camber-free slit edges are critical for high-frequency ERW tube welding. Excessive burr or camber from poor slitting causes weld porosity, edge lap, and premature forming roll wear.

Can one SANSO slitting line process both hot-rolled and galvanized coils?

Yes. By matching arbor diameter, motor torque, and knife clearance shims to material yield strength (up to 550 MPa), a single medium-gauge slitting line processes HR, CR, GI, PPGI, and stainless steel coils.

Start Your Project

Get a Tailored Proposal for Steel Coil Slitting Line (Precision Coil Slitter)

Our engineers design each machine around your coil dimensions, steel grade, and target output.

  • Custom line layout & COPRA roll pass calculation
  • Factory-direct pricing (90% in-house CNC manufacturing)
  • Worldwide on-site installation & commissioning