Executive Engineering Summary: Utility-scale single-axis solar trackers rely on high-torsion square and octagonal torque tubes (typically 100×100 to 150×150 mm, 2.0–4.5 mm wall) manufactured from high-yield pre-galvanized or Zn-Al-Mg (ZAM) coated coils (S350GD–S550GD). SANSO combines scratch-free forming, inline 99.995% pure zinc seam thermal spraying, and burr-free cold sawing to guarantee 25–30 year desert and coastal corrosion resistance.
Solar PV Torque Tube & Racking Specifications
| Solar Component | Coating & Steel Standard | Typical Section & Wall | Critical Manufacturing Challenge |
|---|---|---|---|
| Single-Axis Tracker Torque Tube | ASTM A653 / EN 10346 S350GD–S450GD, Z275 or ZM310 | 100×100, 120×120, 140×140 mm or Octagonal · 2.0–4.5 mm | High springback, strict twist tolerance (≤ 1.0°/m), zero zinc burn-off rust at weld seam |
| Fixed-Tilt PV Purlin & Bracing | Pre-galvanized G90 / Z275 / ZAM | 40×40–80×80 mm & 40×60–50×100 mm · 1.5–3.0 mm | High-volume output with clean punched holes and scratch-free surface finish |
SANSO Solar Tube Mill Line Architecture
| Process Stage | SANSO System | Why It Matters for Solar ZAM / Galvanized Steel |
|---|---|---|
| Master Coil Slitting | High-Precision Steel Coil Slitting Line | Delivers ≤3% edge burr and tight camber control so high-strength S450GD strips track straight through forming. |
| Zero-Flaking Forming | Direct Forming Square / Octagonal Mill | Avoids heavy compressive corner crushing, eliminating zinc/ZAM coating micro-cracking and roll pickup. |
| Weld Seam Anti-Corrosion | 99.995% Pure Zinc Wire + Twin-Wire Arc Seam Sprayer | Immediately restores 15–40 μm metallurgically bonded zinc protection over the scarfed HF weld seam. |
| Thermal-Free Cutting | CNC Flying Cold Saw + TCT Blades | Eliminates friction-saw burn marks that destroy ZAM corrosion protection at tube ends. |
Frequently Asked Questions
Can SANSO mills form octagonal solar tracker torque tubes as well as square tubes?
Yes. SANSO designs custom COPRA RF roll passes for square (SHS), rectangular (RHS), D-profile, and octagonal solar tracker torque tubes, including springback compensation for S450GD–S550GD high-strength steels.
How does SANSO prevent rust along the welded seam of pre-galvanized solar tubes?
Right after OD weld bead scarfing, an inline twin-wire electric arc zinc spraying station applies ultra-pure 99.995% SANSO zinc wire directly onto the hot bare weld line, passing 500–1,000+ hour neutral salt-spray tests (ASTM B117).
Why is a flying cold saw mandatory for ZAM-coated solar profiles?
Abrasive friction saws heat the cut end above 700°C, vaporizing the Zn-Al-Mg coating and leaving heavy melted burrs that cause immediate field corrosion. A CNC flying cold saw cuts cool and burr-free, keeping the ZAM coating intact right up to the cut edge.