Engineering Overview
SANSO HSS Circular Saw Blades and HSS Slitting Saws are CNC-ground from European-grade M2 (DMo5) and M35 (5% Cobalt) high-speed steel, vacuum heat-treated to HRC 64–66, and tensioned for vibration-free cutting on ERW flying cold saws and automatic metal sawing machines. With selectable BW, HZ, and Vario tooth profiles plus VAPO, TiN, TiCN, or TiAlN PVD coatings, they deliver cool, square, burr-free steel tube cuts and can be re-sharpened 15–25 times.
Key Engineering Features & Advantages
- M2 & M35 Cobalt Metallurgy: M2 (DMo5) provides optimal toughness for carbon steel structural tubes; M35 (5% Cobalt) delivers high red-hardness for stainless steel and high-tensile alloy pipes.
- Application-Matched PVD Coatings: Steam-treated VAPO retains coolant for general steel; Gold TiN lowers friction; TiCN & TiAlN resist extreme heat and weld-chip build-up on stainless and high-speed lines.
- Burr-Free HZ & Vario Tooth Geometry: HZ roughing/finishing teeth split chips cleanly on medium-wall tubes, while Vario variable pitch suppresses harmonic chatter on thin-wall tubing (<1.5 mm).
- High Regrind Economy: Full-body high-speed steel construction supports 15–25 CNC resharpening cycles on a SANSO HSS saw blade sharpening machine, lowering cost per cut dramatically.
Technical Specifications
| Steel Grade / Coating | Surface Hardness | Recommended Tube Material | Tooth Forms Available | Standard Diameters |
|---|
| M2 (DMo5) + VAPO Oxide | 900 HV | Low-to-medium carbon ERW tubes | BW, HZ, Vario | Ø250 – Ø450 mm |
| M2 (DMo5) + TiN Gold | 2,300 HV | General carbon & galvanized steel tubes | HZ, Vario | Ø250 – Ø450 mm |
| M35 (Co5) + TiCN / TiAlN | 3,000–3,300 HV | Stainless steel (304/316) & high-tensile pipe | HZ, BW, Vario | Ø250 – Ø500 mm |
| HSS Slitting Saws (M2) | HRC 64–65 | Precision slotting, cutting-off & thin profiles | Form A / B / BW | Ø50 – Ø250 mm |
Process Flow & System Configuration
Match blade grade to steel tensile strength → Select tooth pitch so 2–4 teeth engage wall thickness simultaneously → Apply clean emulsion flood coolant → Resharpen before flank wear exceeds 0.15 mm.
Frequently Asked Questions
How many teeth should an HSS circular saw blade have for thin-wall ERW steel tubes?
For clean burr-free cuts without tooth stripping, 2 to 4 teeth should engage the tube wall thickness at all times. Thin-wall tubes (0.8–1.5 mm) perform best with fine tooth pitch (T4–T5) or Vario variable-pitch geometry.
Should I choose M2 or M35 Cobalt HSS saw blades?
Choose M2 (DMo5) blades for standard carbon and mild steel structural tubing where cost efficiency matters; upgrade to M35 (5% Cobalt) with TiCN or TiAlN coating for stainless steel, alloy tubing, or high-volume cutting.
How many times can a SANSO HSS circular saw blade be resharpened?
When resharpened promptly before excessive flank wear develops, a quality SANSO HSS saw blade can be reground 15 to 25 times using an automatic CNC blade sharpening machine.