Engineering Overview
SANSO TCT Circular Saw Blades (Tungsten Carbide-Tipped & Cermet) are engineered specifically for high-speed ERW tube mill flying cold saws and automated metal sawing machines. Combining laser-cut, precision-tensioned alloy steel bodies with ultra-fine micro-grain carbide or Cermet tips, SANSO TCT blades cut carbon, alloy, and stainless steel tubes up to 3× faster than HSS blades—producing cool, mirror-smooth, burr-free tube ends that eliminate secondary deburring.
Key Engineering Features & Advantages
- Micro-Grain Carbide & Cermet Grades: Sub-micron carbide tips resist chipping on interrupted structural profiles, while titanium-based Cermet tips excel in dry/MQL high-speed cutting of carbon steel pipes with superior surface finish.
- Precision Tensioned SKS51 / 75Cr1 Plate: Laser-cut expansion and damping slots keep the steel plate flat at high RPMs, preventing wander and extending tooth life on flying cold saws.
- Specialized Flying Cold Saw Tooth Grind: Negative/neutral rake triple-chip grind (TCG) and custom chip-breaker grooves eject hot swarf cleanly without welding chips to the blade gullets.
- Lower Total Cost Per Cut: Delivering 4,000 to 12,000+ square meters of cut cross-section per blade, TCT blades slash downtime from blade swaps on 24/7 ERW tube mills.
Technical Specifications
| Blade Diameter (mm) | Kerf / Plate (mm) | Tooth Count (Z) | Bore & Drive Holes | Typical Tube Application |
|---|
| Ø285 / Ø315 | 2.0 / 1.7 | 60 – 100 Z | Ø32 / Ø40 mm | Small ERW25–ERW50 cold saws & thin-wall pipes |
| Ø360 / Ø460 | 2.6 / 2.2 | 72 – 120 Z | Ø50 mm + 4ר16 | Medium ERW76–ERW114 high-speed flying cold saws |
| Ø560 / Ø660 | 3.2 / 2.6 | 90 – 140 Z | Ø60 / Ø80 mm | Heavy ERW165–ERW219 structural & API tube mills |
| Ø800 / Ø1000 | 4.2 / 3.4 | 108 – 160 Z | Custom Flange | Large ERW273–ERW426 heavy-wall flying cold saws |
Process Flow & System Configuration
Confirm flying cold saw spindle RPM & arbor flange → Specify tube steel grade, OD, and wall thickness → Select Cermet (mild/carbon steel) or coated Carbide (stainless/alloy) → Run with MQL mist lubrication for maximum blade life.
Frequently Asked Questions
What is the difference between HSS and TCT saw blades for ERW tube mills?
HSS saw blades run at lower RPMs with flood coolant, resist shock well on older saws, and can be resharpened 15–25 times. TCT/Cermet saw blades run 2–3× faster on modern rigid servo flying cold saws with MQL mist, delivering mirror-smooth burr-free ends and much longer intervals between blade changes.
TCT saw blade price depends on outer diameter (Ø285 mm to Ø1000 mm), carbide vs Cermet tip grade, PVD coating, tooth count, and whether custom flange pinholes or silencer resin slots are required.
Can SANSO match TCT saw blades to non-SANSO flying cold saws?
Yes. Provide your cold saw brand/model or spindle bore, PCD pinhole pattern, diameter, and tube range, and SANSO manufactures direct-fit replacement TCT blades.