Contact Us
ERW Tube Mill

ERW32 Welded Tube Mill Machine (Ø8–32mm)

High-speed ERW32 welded tube mill line engineered for Ø8–32 mm precision round, square, rectangular, and furniture/automotive tubes at speeds up to 130 m/min.

Model / Series
SS-ERW32
Processing Capacity / Range
Round Ø8–32 mm · Square 10×10–25×25 mm
Thickness / Wall Range
0.5 – 2.0 mm
Max Line Speed / Output
Up to 130 m/min
Send Line Specifications
Technical Datasheet

Key Technical Parameters

Specification Item SANSO Engineering Standard
Model / Series SS-ERW32
Processing Capacity / Range Round Ø8–32 mm · Square 10×10–25×25 mm
Thickness / Wall Range 0.5 – 2.0 mm
Max Line Speed / Output Up to 130 m/min
Drive & Power Configuration 100–150 kW Solid-State HF Welder
Applicable Materials / Grade CR / HR / Galvanized Carbon Steel (≤520 MPa)
Precision & Standards Cut Length Tolerance ±1.0 mm · Cold Saw Burr-Free
Primary Applications Furniture tubing, electrical conduits, automotive seat frames, bicycle & fitness tubes

The forming fundamental of ERW tube mill

l The forming fundamental of tube mill: the slit strip is formed into approximate round steel tube without welding by the forming mill,and then the tube’s edge is melted and welded by the HF induction welder  and the welded seam is squeezed Immediately after welding at welding section of tube mill .At this stage, the steel pipe welding is completed, the welded tube through cooling and sizing mill and straightening stand, the final precision steel round or square&rectangular tube is done.

The description

l ERW32 welded tube mill is one model of ERW tube mills .The ERW32 welded tube mill utilizes HF induction welding to manufacture Ø10mm---Ø32mm steel tube and 10X10mm---25x25mm square tube 10X20---20X30mm rectangular tube with the thickness 0.4--2.0mm .

l ERW32 welded tube mill has conventional forming technology, it is ideal for round tube , square&rectangular tube.best control on the tube dimension tolerance and length accuracy.

l For the square and rectangular tube production . We can provide 2 forming processes as option . 

Option1: the steel strip is shaped into round tube by forming machine .after HF welding , the round tube is shaped into square or rectangular tube by sizing machine ,and then the square or rectangular tube is straightened by 2 -Turkeyhead.

ERW32 Welded Tube Mill Machine (Ø8–32mm) - SANSO Machinery

Option2:The steel strip is shaped into round tube by forming machine .after HF welding , the round tube is shaped into square or rectangular tube by 3-Turkey head ,and then the square or rectangular tube is straightened by the 4th -Turkey head .

ERW32 Welded Tube Mill Machine (Ø8–32mm) - technical view 2

One of the forming processes can be determined as per the quantity of square&rectangular and round tube .so that the roller investment can be saved maximum.

l ERW32 welded tube mill is a tailored-made steel tube production line . We are able to design and manufacture the tube mill as per customer’s requirement ,Such as ,the steel tube diameter and thickness , raw material type and raw material yield strength ,specification of tube mill and your floor space dimension,power supply condition .

 Before making quotation ,we will send the customer a request form to customer’s specific requirement. So that we make quotation that completely meet customer’s demand.

l We are not only a provider of tube mill, but also a provider of solution for the problem that arise in the course of Pre-sales, in sales, and after-sales.

The specification

SectionParameterSpecification

Raw Material Specification

The Material

HR/CR carbon steel / Galvanized steel

Width

28mm-100mm

Thickness:

0.4mm-2.0mm

Coil ID

φ450- φ520mm

Coil OD

Max. φ1200mm

Coil Weight

Max.1.2Tons

Tube specification

Round Pipe

10mm-32mm

Square & Rectangular Pipe

8X8mm-25X25mm

10mmX20mm-20mmX30mm

Wall Thickness

0.4–2.0 mm(Round  Pipe)

0.4-1.5mm(Square & Rectangular tube)

Speed of tube mill

Max.140m/min

Pipe Length

3m-12m , can be defined by the customer

The required floor space

50mX5m(L*W)

Total power

250KW

Technological process

Hydraulic Uncoiler→Shear and end welding machine( strip joiner) →Accumulator→forming machine→HF welding  →Eddy current testing →Water Cooling→Sizing machine→ Flying Saw →Run out table→ Packing → Warehouse Storage.

ERW32 Welded Tube Mill Machine (Ø8–32mm) - technical view 3

Our advantage

 1. We have gradually abandoned the idea of designing only two-dimensional drawings. We now design not only two-dimensional drawings but also 3D drawings.

 With advanced 3D modeling and drafting software, allows us to analyze functionality of each part and make any improvements as needed.We can promptly detect design errors.

 2. 31 sets of CNC vertical machining center and 6 sets of CNC horizontal machining center,3 sets CNC boring machine , 2 set of heavy duty CNC gantry milling machine have been in use. This lead to tight accuracy and high productivity, In this way, errors caused by match machining can be avoided, Meanwhile, the delivery time can be ensured.

 2. With the advanced COPRA software , Out engineer not only  calculate  the roller weight  but also design roller at high efficiency.

The application of tube and hollow profile

The ERW tubes and profiles produced by the pipe mill can be utilized in the industry below:

l Metal Furniture: Frames and support structures for chairs, tables, bed frames, sofas, coat racks, and bookshelves.

l Outdoor Furniture: Armrests and brackets for park benches and beach chairs.

l Fitness Equipment: Frames for home or light commercial fitness equipment, such as treadmills, elliptical trainers, exercise bikes, and parallel bars.

l Medical Equipment: Brackets and handles for wheelchairs, hospital beds, IV poles, and carts.

l Mechanical Equipment: Frames, ventilation ducts, and protective covers for various light mechanical equipment.

l Decoration and Art:Indoor and Outdoor Decoration: Decorative guardrails, screens, partitions, display racks, and supermarket shelves.

l Bicycles and Motorcycles: Components such as handlebars, subframes, and luggage racks.

l Automobiles: Interior support, ventilation ducts, and wiring harness protection.

l Display and Storage Equipment:display racks: Merchandise display racks and booth frames in shopping malls and showrooms.

l Shelves: Lightweight storage racks, bookshelves, shoe racks, etc.

Frequently Asked Questions About SS-ERW32

What pipe sizes and thicknesses can the SANSO SS-ERW32 produce?

The SANSO SS-ERW32 high-frequency welded tube mill manufactures Round Ø8–32 mm · Square 10×10–25×25 mm steel pipes with wall thicknesses of 0.5 – 2.0 mm at production speeds up to Up to 130 m/min, supporting round, square, and rectangular structural or fluid-transport profiles.

Does SANSO manufacture the SS-ERW32 forming stands and gearboxes in-house?

Yes. Approximately 90% of SANSO SS-ERW32 mechanical components—including bases, arch stands, shafts, and precision gears—are CNC machined in-house at our Shijiazhuang factory and cold-commissioned prior to shipment for rapid on-site installation.

What auxiliary equipment is included in a turnkey SS-ERW32 production line?

A complete turnkey SS-ERW32 line integrates a hydraulic or double-head uncoiler, strip shear & end welder, horizontal spiral or cage accumulator, forming & sizing mill, solid-state HF welder, coolant filtration & impeder assembly, inline eddy current testing (optional), computerized flying cold saw, and automatic pipe packing machine.

Start Your Project

Get a Tailored Proposal for ERW32 Welded Tube Mill Machine (Ø8–32mm)

Our engineers design each machine around your coil dimensions, steel grade, and target output.

  • Custom line layout & COPRA roll pass calculation
  • Factory-direct pricing (90% in-house CNC manufacturing)
  • Worldwide on-site installation & commissioning