Engineering Overview
SANSO Pure Zinc Wire (≥99.995% Zn, Special High Grade) is drawn specifically for inline weld-seam zinc spraying on pre-galvanized ERW steel tube mills. After high-frequency welding and OD scarfing burn off the galvanized coating along the weld line, SANSO pure zinc wire feeds smoothly through twin-wire electric arc spray guns to restore dense, bright, corrosion-resistant zinc protection that matches the parent galvanized pipe.
Key Engineering Features & Advantages
- Ultra-High 99.995% Purity (SHG): Low impurity levels (Pb ≤0.002%, Fe ≤0.001%, Cd ≤0.001%) ensure smooth arc atomization, uniform molten droplet size, and superior salt-spray corrosion resistance.
- Zero-Kink Layer-Wound Packaging: Precision layer-wound 15–25 kg spools and 200–250 kg heavy pay-off drums guarantee continuous, snag-free feeding during 24/7 galvanized pipe runs.
- Consistent Tensile & Diameter Control: Tight ±0.03 mm diameter control and controlled temper prevent wire bird-nesting inside drive rollers and contact tips.
- Complete Seam-Spraying Support: Supplied alongside SANSO inline arc-spray zinc metallizing units, fume extractors, and weld-seam polishing brushes for turnkey galvanized tube production.
Technical Specifications
| Chemical / Physical Property | SANSO Specification | Standard Reference |
|---|
| Zinc Purity (Zn) | ≥ 99.995% | ASTM B6 SHG / EN 1179 Z1 |
| Standard Wire Diameters | 1.6 mm, 2.0 mm, 2.5 mm, 3.0 mm | Tolerance ±0.03 mm |
| Tensile Strength | 110 – 145 MPa | Optimized for push-pull arc guns |
| Elongation | ≥ 35% | Prevents brittle snapping on payoff |
| Packaging Options | 15 / 20 / 25 kg Spools · 100 / 200 / 250 kg Drums | Moisture-barrier vacuum sealed |
Process Flow & System Configuration
HF Welding of Pre-Galvanized Strip → OD Scarfing → Inline Twin-Wire Arc Spraying with 99.995% Pure Zinc Wire → Air Cooling & Seam Polishing → Salt-Spray Verified Corrosion Protection.
Frequently Asked Questions
How much pure zinc wire is consumed per ton of galvanized ERW steel tube?
Typical inline weld-seam spraying uses roughly 0.8 kg to 1.8 kg of pure zinc wire per ton of finished galvanized pipe, depending on pipe diameter, wall thickness, scarfed seam width, and target coating thickness (typically 15–30 μm).
What wire diameter is most common for ERW tube mill zinc spraying?
Ø2.0 mm and Ø2.5 mm pure zinc wire in 200 kg payoff drums are the most popular choices for continuous ERW tube mills, balancing high deposition rate with minimal spool changeover downtime.
Pure zinc wire pricing tracks the LME/SHFE Special High Grade (SHG) zinc ingot benchmark plus precision wire drawing, spool/drum packaging, and order volume (MOQ typically 1 ton or bundled with equipment shipments).