Engineering Overview
The SANSO Online Eddy Current Testing (ECT) System performs 100% continuous non-destructive inspection of ERW welded tubes directly on the mill line at speeds up to 150 m/min. Equipped with multi-frequency digital signal processing, DC magnetic saturation to suppress carbon-steel permeability noise, and automatic paint-spray marking and sorting triggers, it instantly detects open seams, pinholes, cracks, and cold welds before cutting.
Key Engineering Features & Advantages
- 100% Inline Weld Seam Verification: Detects pinholes, longitudinal cracks, open welds, weld skips, and surface inclusions instantaneously—alerting operators immediately to correct HF welding drift before producing scrap.
- DC Magnetic Saturation Unit: Saturates ferromagnetic carbon steel tubes magnetically during inspection to eliminate permeability noise and achieve crisp signal-to-noise ratios compliant with ASTM E309 and API 5L.
- Encircling & Saddle Sector Coils: Full-circumference encircling coils inspect Ø8–165 mm tubes; targeted saddle weld-seam probes inspect large-diameter and square/rectangular sections up to 508 mm.
- Automated Defect Tracking & Sorting: PLC encoder tracks every flagged defect through the flying saw to trigger automatic paint spray marking and pneumatic reject sorting on the runout table.
Technical Specifications
| Model | Pipe OD Range | Probe Type | Frequency Range | Compliance Standards |
|---|
| SS-ECT76 | Ø8 – Ø76 mm | Encircling + DC Saturation | 1 kHz – 500 kHz | ASTM E309 / EN ISO 10893-2 |
| SS-ECT165 | Ø32 – Ø165 mm | Encircling or Sector Saddle | 1 kHz – 500 kHz | ASTM E309 / API 5L / GB/T 7735 |
| SS-ECT508 | Ø114 – Ø508 mm | Dedicated Weld-Seam Saddle | 1 kHz – 300 kHz | API 5L / EN ISO 10893-2 |
Process Flow & System Configuration
Post-Sizing Tube Entry → Guide Roller Alignment → DC Magnetic Saturation Coil → Multi-Frequency Eddy Current Inspection Coil → Real-Time Digital Impedance Plane Analysis → Paint Spray Marker & Automated Reject Gate Signal.
Frequently Asked Questions
Where is an eddy current testing unit installed on an ERW tube mill?
The eddy current testing stand is installed immediately after the sizing mill and cooling trough (upstream of the Turks head or flying saw) where pipe geometry is stable and temperature is below 60°C.
Why is magnetic saturation required for eddy current testing of carbon steel ERW tubes?
Carbon steel is ferromagnetic with localized permeability variations around the heat-affected weld zone. A DC magnetic saturation unit drives the steel into magnetic saturation so permeability noise disappears and genuine cracks or pinholes stand out cleanly.
What international standards do SANSO tube eddy current inspection systems meet?
SANSO inline ECT systems calibrate against standard drilled-hole and EDM-notch reference tubes meeting ASTM E309, ASTM E426, API 5L, EN ISO 10893-2, and GB/T 7735 requirements.