Contact Us
Cored Wire Production Line

Solid Calcium Cored Wire Production Line (SS-10)

Turnkey SS-10 solid pure calcium cored wire forming line producing Ø9–13.5 mm seamless steel-clad calcium wire for clean steel ladle metallurgy and refining.

Model / Series
SS-10 Solid Calcium Line
Processing Capacity / Range
Finished Wire OD Ø9.0 – Ø13.5 ± 0.5 mm
Thickness / Wall Range
Steel Strip Thickness 0.4 – 1.0 mm
Max Line Speed / Output
30 – 60 m/min
Technical Datasheet

Key Technical Parameters

Specification Item SANSO Engineering Standard
Model / Series SS-10 Solid Calcium Line
Processing Capacity / Range Finished Wire OD Ø9.0 – Ø13.5 ± 0.5 mm
Thickness / Wall Range Steel Strip Thickness 0.4 – 1.0 mm
Max Line Speed / Output 30 – 60 m/min
Drive & Power Configuration Synchronized Strip & Calcium Core Roll Forming + Recoiler
Applicable Materials / Grade Low-Carbon Cold-Rolled Strip + Pure Solid Calcium Core
Precision & Standards Tight Interlocked Seam · Uniform Calcium/Steel Ratio
Primary Applications Ladle metallurgy desulfurization, calcium treatment & inclusion modification in steelmaking
Live Workshop Demonstration

Solid Calcium Cored Wire Production Line (SS-10) — Running Video

All Machine Videos →

See SANSO Precision in Real Production

Turnkey SS-10 solid pure calcium cored wire forming line producing Ø9–13.5 mm seamless steel-clad calcium wire for clean steel ladle metallurgy and refining.

  • Actual factory trial run & cold-commissioning footage from SANSO Shijiazhuang workshop
  • Demonstrates forming alignment, line speed stability, and automated control operation
  • Need custom tube OD, wall thickness, or steel grade test video? Request a tailored workshop demo

1 The definition of solid calcium cored wire production line

Solid calcium cored wire production line is a specialized metallurgical equipment. Its core function is to tightly wrap high-purity calcium metal wire with a steel strip, continuously producing solid calcium cored wire for steel making applications.

2 Process Flow of the Seamless Solid Calcium Cored Wire Line

The standard process flow of the seamless solid calcium cored wire production line is as follows:

Steel coil uncoiler → Shear and end welder → Calcium wire uncoiler → Cage accumulator → Preforming machine → Calcium wire feeding unit → HF welder → Calibration machine → Solid calcium cored wire laying unit → Rewinder → Unloading car

Each section has a clear function in the production process.

3 Main Production Sections

solid-calcium-cored-wire-production-line-1

(1)Steel Coil Uncoiler

1-Uncoiler

The steel coil uncoiler supports and releases the steel strip used as the outer sheath of the cored wire. Stable strip feeding is important because the following forming and welding sections depend on continuous and even material supply.

(2)Shear and End Welder

2-Shear and end welder

The shear and end welder is used to cut and join the strip ends. This helps reduce production interruption when changing coils and keeps the production line running more continuously.

(3)Calcium Wire Uncoiler

3- calcium wire uncoiler

The calcium wire uncoiler releases the solid calcium wire used as the filler. Smooth calcium wire feeding is important because the filler needs to enter the formed steel strip accurately before HF welding.

(4)Cage Accumulator

4-Cage accumulator

The cage accumulator stores strip material temporarily and helps balance the production rhythm between coil changing and continuous line operation. It is useful for improving production continuity and reducing frequent line stoppage.

(5)Preforming Machine

5-preforming machine

The preforming machine gradually shapes the steel strip before the calcium wire is fully enclosed. Proper preforming helps the strip wrap around the calcium wire smoothly and prepares the wire for stable seam welding.

(6)Calcium Wire Feeding Unit

6-calcium wire feeding unit

The calcium wire feeding unit guides the calcium wire into the formed steel strip. This section must keep the filler position stable, because poor feeding may affect the final wire structure and sealing quality.

(7)HF Welder

7-HF welder

The HF welder seals the steel strip seam to form a seamless-type solid calcium cored wire. High-frequency welding is used to close the seam and create a stable outer sheath around the calcium wire.

(8)Calibration Machine

8-calbrication machine

The calibration machine is used to control the final wire shape and diameter after welding. This helps improve dimensional consistency and makes the finished cored wire easier to rewind, handle, and use in later wire feeding applications.

(9)Solid Calcium Cored Wire Laying Unit

9-cored wire laying unit

The laying unit arranges the finished wire before rewinding. Stable laying helps avoid uneven winding and supports better coil quality.

(10)Rewinder and Unloading Car

10-Rewinder+

The rewinder collects the finished solid calcium cored wire into coils. The unloading car helps move the finished coil away from the rewinding section for packaging, storage, or further handling.

4 The video of solid calcium cored wire


Specification of Seamless Solid Calcium Cored Wire

The following specifications are based on the customer’s provided product information:

(1)The steel trip thickness :1.0---1.5mm

(2)The solid cored wire diameter :9.5mm,10.5mm ( dimension accuracy:±0.5mm)

(3)The filler : Calcium wire

(4)Seal type :HF welding(seamless type) 

(5)Application:steel making

solid-calcium-cored-wire-production-line-11

The actual line configuration can be discussed according to the buyer’s required wire diameter, strip thickness, filler type, production speed, coil size, and application requirements.

Applications of Solid Calcium Cored Wire

Solid calcium cored wire is mainly used in steelmaking and foundry applications. In steel plants, it is commonly used during secondary refining and calcium treatment.

(1)Refining the molten steel: Deep deoxidation and desulfurization to remove harmful inclusions.

(2)Optimizing the microstructure: Modifying inclusion morphology to enhance the comprehensive mechanical properties of the steel.

(3)Ensuring smooth production: Solving the problem of tundish nozzle clogging during continuous casting to guarantee production continuity.

(4)Improving cost-effectiveness: Compared with traditional methods, it offers higher elemental yield, more stable treatment performance, and lower overall costs.

This technology is an indispensable key process for producing high-quality steel grades, such as pipeline steel, automotive steel, and other critical applications.

solid-calcium-cored-wire-production-line-12


Frequently Asked Questions

What wire diameter and seam accuracy does the SANSO SS-10 Solid Calcium Cored Wire Machine deliver?

The SS-10 produces metallurgical solid pure calcium cored wire at Ø13.5 ± 0.5 mm (1.0 mm steel sheath) with a tight, moisture-sealed double-lock seam for reliable steelmaking ladle injection.

Does SANSO supply complete turnkey cored wire lines including recoiling and payoff systems?

Yes. Each turnkey line integrates coil payoff, roll-forming stands, calcium core feeding, lock-seaming, length counter, and automatic horizontal/vertical cage spooler.

Start Your Project

Get a Tailored Proposal for Solid Calcium Cored Wire Production Line (SS-10)

Our engineers design each machine around your coil dimensions, steel grade, and target output.

  • Custom line layout & COPRA roll pass calculation
  • Factory-direct pricing (90% in-house CNC manufacturing)
  • Worldwide on-site installation & commissioning